Investigation of the effect of the addition of grain refiner and modifier addition on wear properties in sand and permanent mould casting of A357 and A380 aluminium alloys

MakaleYalnız künyeScopus SJRQ2

Özet

The aim of this study is to improve the tribological behaviour of aluminium alloys by using grain refiner and modifier. The effects of Al5Ti1B grain refiner and Al10Sr modifier additives on friction and wear properties on A380, A357 alloys produced by pouring sand andpermanent mould casting were investigated. Abrasion tests were carried out under dry conditions against St1040 steel disc using a pin-disk system with 20 N load and 1.0 m/s sliding speed. It was determined that grain refiner and modifier additives decrease the friction coefficient and increase the wear resistance. It was determined that the samples produced by permanent mould casting method decreased the friction resistance by 9% and the abrasion resistance increased by 40% compared to the samples produced in sand mould. The lowest wear rate was obtained in A380 alloy with TiB and Sr added with a value of 4.87 × 10–11 m2/N.

Anahtar Kelimeler

RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/bayburt/13369Resmi atıflarda kullanılan kalıcı adres
İndeks kayıtları
Kaydın indeks veri tabanlarındaki sayfası (aktarımda alınan kayıt numarasıyla). Erişim, indeksin kendi koşullarına bağlıdır.
Atıflar
Scopus
12
WoS
10
OpenAlex
13
Her kaynağın kendi saydığı toplam atıf; aktarım ve zenginleştirme sırasında alındı.
Tam Kayıt
AlanDeğerDil
dc.contributor.authorÇolak, Murat
dc.contributor.authorArslan, İbrahim
dc.date.accessioned2026-10-29T19:10:51.484205850Z
dc.date.available2026-10-29T19:10:51.484205850Z
dc.date.issued2022
dc.description.abstractThe aim of this study is to improve the tribological behaviour of aluminium alloys by using grain refiner and modifier. The effects of Al5Ti1B grain refiner and Al10Sr modifier additives on friction and wear properties on A380, A357 alloys produced by pouring sand andpermanent mould casting were investigated. Abrasion tests were carried out under dry conditions against St1040 steel disc using a pin-disk system with 20 N load and 1.0 m/s sliding speed. It was determined that grain refiner and modifier additives decrease the friction coefficient and increase the wear resistance. It was determined that the samples produced by permanent mould casting method decreased the friction resistance by 9% and the abrasion resistance increased by 40% compared to the samples produced in sand mould. The lowest wear rate was obtained in A380 alloy with TiB and Sr added with a value of 4.87 × 10–11 m2/N.
dc.identifier.doi10.1080/13640461.2022.2069912
dc.identifier.eissn1743-1336
dc.identifier.endpage23
dc.identifier.issn1364-0461
dc.identifier.issue1-3
dc.identifier.scopus2-s2.0-85129845882
dc.identifier.startpage17
dc.identifier.urihttps://rdlopen.rawdatalibrary.net/r/bayburt/13369
dc.identifier.volume35
dc.identifier.wosWOS:000794296800001
dc.language.isoen
dc.publisherTaylor and Francis Ltd.
dc.relation.ispartofInternational Journal of Cast Metals Research
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectAluminium casting
dc.subjectgrain refinement
dc.subjectmodification
dc.subjectpermanent mould casting
dc.subjectsand casting
dc.subjectwear
dc.subject.classificationMetallurgy & Metallurgical Engineering
dc.subject.otherAbrasion
dc.subject.otherAluminum alloys
dc.subject.otherBinary alloys
dc.subject.otherErosion
dc.subject.otherFriction
dc.subject.otherMolds
dc.subject.otherRefining
dc.subject.otherSand
dc.subject.otherTribology
dc.subject.otherWear resistance
dc.subject.otherFriction and wear properties
dc.subject.otherGrain refiner
dc.subject.otherGrains refinement
dc.subject.otherModification
dc.subject.otherModifier addition
dc.subject.otherRefiner addition
dc.subject.otherSand mold
dc.subject.otherSand-castings
dc.subject.otherTribological behaviour
dc.subject.otherWear properties
dc.subject.otherGrain refinement
dc.titleInvestigation of the effect of the addition of grain refiner and modifier addition on wear properties in sand and permanent mould casting of A357 and A380 aluminium alloys
dc.typeArticle
rdl.citation.openalex13
rdl.citation.scopus12
rdl.citation.wos10
rdl.oa.statusclosed
rdl.scopus.quartileQ2
rdl.source.indexSCOPUS
rdl.source.indexWOS
rdl.wos.indexScience Citation Index Expanded (SCI-EXPANDED)